Key Takeaways

  • Adding a small amount of biochar made from waste sugarcane husks strengthens plant-based plastics while making them much harder to burn.
  • Natural fiber materials are lightweight and renewable, yet they typically catch fire easily and lack the durability required for heavy industrial parts.
  • Mixing an exact balance of sugarcane biochar into flax and kenaf layered resin produces peak strength, stiffness, and resistance to heat.
  • Adding too much biochar causes tiny particles to clump together, which weakens the final material and reduces its protective fire barrier.
  • Researchers successfully shaped this improved plant-based material into a sturdy pipe prototype suitable for future electrical conduit testing.

In a new study published in Scientific Reports, researchers G. Velmurugan, Jasgurpreet Singh Chohan, S. A. Muhammed Abraar, K. Velusamy, D. Elil Raja, Ramya Maranan, K. Arunprasath, Arun Kumar, and Regasa Yadeta Sembeta evaluated how adding sugarcane biochar affects the structural strength and fire safety of plant-fiber plastics. While engineers increasingly favor renewable plant fibers like flax and kenaf to reduce weight in industrial parts, these natural materials burn easily and lose strength at high temperatures. By mixing carbon-rich biochar derived from waste sugarcane husks into layered flax and kenaf epoxy composites, the research team sought to create a durable, fire-resistant material capable of serving in demanding applications such as electrical conduit pipes.

The mechanical testing revealed a clear optimal concentration for the biochar additive. When the researchers tested composites containing between zero and six percent sugarcane biochar by weight, every major strength metric improved steadily up to a loading of 4.5 percent. Compared to plain epoxy resin, the 4.5 percent biochar composite achieved a 73.7 percent increase in tensile strength, reaching 38.01 megapascals, alongside a flexural strength of 76.12 megapascals. Impact resistance more than tripled compared to plain epoxy, rising to 9.62 kilojoules per square meter, while surface hardness reached 86 on the Shore D scale and interlaminar shear strength climbed to 13.24 megapascals. Only elongation at break peaked earlier, reaching its highest flexibility at a three percent biochar loading before stiffening at higher concentrations.

Thermal and flammability evaluations demonstrated that the 4.5 percent biochar formulation also delivered the strongest resistance to fire. During thermal degradation testing, the temperature at which the material began breaking down rose by 39 degrees Celsius over plain epoxy to reach 317 degrees Celsius. Furthermore, the amount of stable char remaining after extreme heating rose from 11 percent in plain epoxy to 28 percent in the optimized composite. In direct fire tests, the limiting oxygen index increased from 19.5 percent to 28.4 percent, meaning the material required a much higher concentration of oxygen to sustain a flame. Ignition time nearly doubled from 32 seconds to 61 seconds, while peak heat release rate dropped by 42.3 percent to 300.10 kilowatts per square meter and total heat release fell by 30.7 percent. Horizontal burning rates also slowed from 3.8 millimeters per minute down to 2.1 millimeters per minute.

Microscopic examination explained both the performance peak at 4.5 percent and the subsequent decline observed when biochar loading reached six percent. At 4.5 percent, the biochar particles dispersed evenly throughout the epoxy resin, anchoring the flax and kenaf fibers tightly and minimizing structural voids. When exposed to flame, this uniform distribution helped form a dense, continuous layer of protective char on the surface that slowed heat transfer and restricted combustible gases. However, pushing the biochar content to six percent caused particles to clump together, creating weak spots that reduced mechanical strength and disrupted the protective char layer during burning.

To demonstrate practical manufacturing feasibility, the researchers molded the optimized 4.5 percent biochar composite into a cylindrical electrical conduit prototype measuring 300 millimeters in length with a three-millimeter wall thickness. The molded pipe retained sound dimensional stability, proving that agricultural waste products like sugarcane husks, flax, and kenaf can be processed into complex structural shapes. The authors note that before this bio-based composite can replace conventional polyvinyl chloride pipes in commercial installations, future testing must verify its electrical insulation properties, moisture resistance, and compliance with standard conduit safety certifications.


Source: Velmurugan, G., Chohan, J. S., Abraar, S. A. M., Velusamy, K., Raja, D. E., Maranan, R., Arunprasath, K., Kumar, A., & Sembeta, R. Y. (2026). Development of flax/kenaf hybrid epoxy composites incorporating sugarcane biochar with enhanced fire performance for potential electrical conduit applications. Scientific Reports, Article in Press.


Leave a Reply